Skip to main navigation Skip to search Skip to main content

Microstructure, cryogenic tensile and fracture behavior of laser welded Co17.5Cr12.5Fe55Ni10Mo5 complex concentrated alloy

  • Jae Hyuk Lee
  • , Jeongmin Lee
  • , Hidemi Kato
  • , Seungkyun Yim
  • , Dongkyoung Lee
  • , Gian Song
  • , Jeong Hun Lee
  • , Dong Jun Lee
  • , Young Kyun Kim
  • , Young Sang Na
  • , Hyoung Seop Kim
  • , Jongun Moon
  • , Soo Hyun Joo*
  • *Corresponding author for this work
  • Dankook University
  • Kongju National University
  • Tohoku University
  • Kyungpook National University
  • Korea Institute of Materials Science
  • Pohang University of Science and Technology

Research output: Contribution to journal › Journal article › peer-review

Abstract

This study investigates the microstructural evolution, cryogenic deformation behavior, and residual stress of butt laser-welded Co17.5Cr12.5Fe55Ni10Mo5 complex concentrated alloy (CCA). Two laser welding parameter sets—15 mm/s at 0.6 kW and 20 mm/s at 0.7 kW—were optimized through preliminary bead-on-plate experiments, achieving full penetration without macroscopic geometric defects, and yielding pore volume percentages of 0.0092% and 0.0677%, respectively, as quantified by X-CT. Both welding conditions resulted in columnar grains in the fusion zone (FZ), exhibiting a pronounced <001> crystallographic texture oriented perpendicular to the welding direction, accompanied by cellular substructures. Quantitative analysis revealed that the 15 mm/s at 0.6 kW condition produced a higher μ-phase area percentage of 7.0% together with finer cellular features, which correlated with higher hardness values of approximately 200–250 HV in the FZ. Additionally, this condition resulted in a ∼7.3-fold lower total pore volume compared to the 20 mm/s at 0.7 kW condition, as confirmed by micro-computed tomography. Tensile testing revealed reduced joint efficiency relative to the base alloy, with yield strength, ultimate tensile strength, and total elongation efficiencies of 81.1–86.0%, 74.3–92.3%, and 29.6–70.6%, respectively, primarily due to the presence of micropores, coarse grain formation, and suppressed deformation-induced martensitic transformation (DIMT). Moreover, residual stress analysis showed transverse tensile stresses exceeding 200 MPa near the weld center. Nevertheless, the 15 mm/s at 0.6 kW condition demonstrated reasonable cryogenic mechanical performance, attributed to more active DIMT.

Original languageEnglish
Article number150106
JournalMaterials Science and Engineering: A
Volume960
DOIs
StatePublished - 2026.05
Externally publishedYes

Keywords

  • Butt laser welding
  • CoCrFeNiMo
  • Complex concentrated alloy
  • Cryogenic deformation
  • Deformation-induced martensitic transformation
  • Residual stress

Fingerprint

Dive into the research topics of 'Microstructure, cryogenic tensile and fracture behavior of laser welded Co17.5Cr12.5Fe55Ni10Mo5 complex concentrated alloy'. Together they form a unique fingerprint.