Abstract
Fluorinated dihydroxy phosphine oxide monomers were synthesized via chlorination, Grignard, and demethylation techniques. The prepared monomer was successfully polymerized with each of the three perfluorinated monomers (decafluorobiphenyl, decafluorobenzophenone, and pentanuorophenylsulfide) by nucleophilic aromatic substitution. The average molecular weight ranged between 7800 and 14,900 g/mol. The glass-transition temperatures of the polymers were registered in the range of 185-235 °C, and all the polymers exhibited high thermal stability up to 326-408 °C. The results of the refractive-index measurements indicated control of the refractive index between 1.5181 and 1.5536 and an optical loss of 0.53 dB/cm at 1550 nm.
| Original language | English |
|---|---|
| Pages (from-to) | 1497-1503 |
| Number of pages | 7 |
| Journal | Journal of Polymer Science, Part A: Polymer Chemistry |
| Volume | 41 |
| Issue number | 10 |
| DOIs | |
| State | Published - 2003.05.15 |
Keywords
- Halogenated
- Optical loss
- Poly(arylene ether phosphine oxide)
- Refractive index
- Step-growth polymerization
Fingerprint
Dive into the research topics of 'Synthesis and optical properties of fluorinated poly(arylene ether phosphine oxide)s'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver