The effect of ultrasonic melt treatment on the microstructure and mechanical properties of Al-7Si-0.35Mg casting alloys

  • Soo Bae Kim
  • , Young Hee Cho
  • , Jung Moo Lee*
  • , Jae Gil Jung
  • , Su Gun Lim
  • *Corresponding author for this work
  • Korea Institute of Materials Science
  • Gyeongsang National University

Research output: Contribution to journal › Journal article › peer-review

Abstract

The effect of ultrasonic melt treatment (UST) on the microstructure and mechanical properties of Al-7Si-0.35Mg (A356) casting alloys was investigated. The particular aim of this study was to analyze the mechanism involved in the strengthening of the A356 alloys when fabricated by UST. The UST had little effect on the sizes of the α-Al grain and eutectic Si at a melt temperature of 750 °C, and the yield strength of the A356 alloy was increased by UST by approximately 16%. After T6 heat treatment, however, both alloys prepared with and without UST had similar levels of yield strength. These results are possibly associated with a change in the type and the volume fraction of intermetallics due to UST. UST greatly reduced the volume fractions of the intermetallics which were formed upon solidification, resulting in alloys with predominantly β-Al5-FeSi instead of π-Al8FeMg3Si6. However, T6 heat treatment, especially a solid solution treatment at 530 °C for 8 hours, led to the dissolving of intermetallics such as Mg2Si and π-Al8FeMg3Si6 and as a result their volume fractions were further reduced to similar levels in both alloys with and without UST.

Original languageEnglish
Pages (from-to)240-246
Number of pages7
JournalJournal of Korean Institute of Metals and Materials
Volume55
Issue number4
DOIs
StatePublished - 2017.04

Keywords

  • Casting
  • Hypoeutectic Al-Si alloy
  • Mechanical properties
  • Microstructure
  • Ultrasonic melt treatment